plastic stool injection mould
The parting line of the chair mold is very important. How to control the edge without burrs and flash, then the first design is very important. Whether the mold wall thickness of the core cavity is sufficient.
Secondly, for the core cavity, the mold processing is very important. Some companies process it once, while others process it twice, but under normal circumstances we need to process it three times. From the roughening of the steel material to the quenching and tempering and nitriding, we then carry out the second program of numerical control. The previous general stage is called semi-finishing. Under normal circumstances, at this stage of processing, we will reserve a machining allowance of 0.3mm and wait for the steel stress to be fully released before we perform finishing.
Machining accuracy at this time is very important. First, after CNC milling, the steel must be initially cooled. During reprocessing, the cutting depth should not be greater than 0.08mm each time. These are to prevent deformation caused by CNC milling and quenched and tempered steel. Such strict control of each process can ensure a perfect parting line.
1. The mold material is made of high-quality steel.
2. Use world-class 3D modeling software to design the shape of the plastic bottle.
3. A variety of plastic bottle shape suggestions can be provided.
4. The mold shows chrome plating.
5. Reasonable cooling water channel design.
6. The parts are processed by cnc equipment
We will meet your needs in tooling builds and injection molding, rapid
scale up ramps for initial market launch, and full-scale manufacturing.
Our
focus is on innovative products and specialized in shortening the time
between development time and manufacturing for our customer.